dc.description.abstractIn this project, a study of creep mechanism in an Al-2.25 wt % Mg alloy is conducted at temperatures between 573K and 623K and stresses (α ) ranging from 7.70 to 48.10 Mpa. Using the dislocation network model, the characteristics features of recovery-controlled and glidecontrolled creep mechanisms are delineated. One of the manifestations of the fundamental differences between these two mechanisms, it is demonstrated, is the disparity which should be observed between the experimentally observed obstacle strength parameter α exp in the equation σ = α exp Gb/p where G, b and p are the shear modulus, the Burgers vector of dislocations and the dislocation density respectively and the theoretically calculated value, αo. Specifically, the theoretical model predicts that α exp for glide creep should be greater than α exp for recovery creep. The conditions under which a transition from one creep mechanism to the other could occur in a given material are investigated (theoretically). It is demonstrated that for creep to be glidecontrolled, the dislocation glide velocity Vg must be related to the annihilation rate p a according to the expression Vg << β p a / (α1 p 3/2). Where α1 and β are constants. Otherwise, creep should be recovery-controlled. The implications of the theoretical model on the shape of creep curves for both mechanisms are discussed and are shown to be generally consistent with literature data. The creep tests performed on the Al-Mg alloy show that inverse transient creep curves are observed at low stresses and normal transients at high stresses. Also a change in transient creep curve shapes are observes when the annealed samples are prestrained prior to creep. Stress increase and stress removal tests performed (in the high stress range) during creep reveal certain creep characteristics which are trademarks of recovery-controlled creep at high stresses. Recovery tests performed on prestrained samples show that the flow stress decreases with recovery time, even though it never quite approaches the value characteristics of annealed samples.en_US
dc.identifier.citationFagbulu J.B (1985) Creep studies in aluminium-2.25WT.% magnesium.en_US
dc.identifier.urihttps://ir.oauife.edu.ng/123456789/5354
dc.language.isoenen_US
dc.publisherObafemi Awolowo Universityen_US
dc.subjectElementsen_US
dc.subjectDislocation network modelen_US
dc.subjectBurgers vector/en_US
dc.subjectAnnealed samplesen_US
dc.titleCreep Studies in Aluminium-2.25WT.% Magnesium.en_US
dc.typeThesisen_US
Files
Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
Creep studies in aluminium-2.25WT.% magnesium-M.Sc.pdf
Size:
99.62 KB
Format:
Adobe Portable Document Format
Description:
M.Sc. Engineering Physics Department of Physics
License bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
license.txt
Size:
1.71 KB
Format:
Item-specific license agreed upon to submission
Description:
Collections